High Temperature 3D Printing Spherical Powder Incoloy 800 Forgings Pipes Tubes Bars Plates Sheets Strips Wires Rods

Incoloy 800 series of alloy (Incoloy 800, 800H and 800HT) are nickel-iron-chromium superalloys that have excellent properties of high temperature strength and resistance to oxidation, carburization and other types of high temperature corrosion. Incoloy 800, 800H and 800HT are used in various applications from furnace components, petrochemical furnace cracker tubes to sheathing for electrical heating elements.

Description

High Temperature 3D printing spherical powder Incoloy 800 Forgings pipes tubes bars plates sheets Strips wires Rods


We are leading manufacturer and stockiest of Incoloy 800 in China.


Incoloy 800 Technical Data Sheet


Incoloy 800 Chemical Composition Limits

Weight %

Ni

Cr

Fe

C

Al

Ti

Al+Ti

Alloy 800

30-35

19-23

39.5 min

0.10 max

0.15-0.60

0.15-0.60

0.30-1.20

Alloy 800H

30-35

19-23

39.5

0.05-0.10

0.15-0.60

0.15-0.60

0.30-1.20

Alloy 800HT

30-35

19-23

39.5

0.06-0.10

0.25-0.60

0.25-0.60

0.85-1.20


Incoloy 800 series of alloy (Incoloy 800, 800H and 800HT) are nickel-iron-chromium superalloys that have excellent properties of high temperature strength and resistance to oxidation, carburization and other types of high temperature corrosion. Incoloy 800, 800H and 800HT are used in various applications from furnace components, petrochemical furnace cracker tubes to sheathing for electrical heating elements.


Incoloy 800 Mechanical Properties


Material

Temp

Hardnes BHN

Tensile Strength MPa

Yield Strength (0.2% Offset)

 

F

C

 

ksi

MPa

ksi

MPa

Alloy 800H and Alloy 800HT

80

27

126

77.8

536

21.7

150

Alloy 800H and Alloy 800HT

800

425

 

67.5

465

18.8

130

Alloy 800H and Alloy 800HT

1000

540

90

62.7

432

13.0

90

Alloy 800H and Alloy 800HT

1200

650

84

54.8

378

13.5

93

Alloy 800H and Alloy 800HT

1300

705

82

47.7

329

15.8

109

Alloy 800H and Alloy 800HT

1400

760

74

34.2

236

13.1

90


Incoloy 800 Specifications

Alloy 800 - UNS N08800

Alloy 800H - UNS N08810

Alloy 800HT - UNS N08811


Rod

ASTM B 408, ASME SB 408, ISO 9723, BS 3076NA15, DIN 17460, EN 10095

Bar

AMS 5766,ASTM B 408, ASME SB 408, ISO 9723, BS 3076NA15, DIN 17460, EN 10095

Wire

ISO 9724, BS 3075NA15

Forgings

AMS 5766, ASTM B564, ASME SB 564, ASME Code Case 1949, ISO 9725, DIN 17460

Plate

AMS 5871, ASTM A 240/A 480, ASME SA 240/SA 480, ASTM B 409/B 906, ASME SB 409/SB 906, BS 3072NA15, DIN 17460, EN 10028-7, EN 10095

Sheet

AMS 5871, ASTM A 240/A 480, ASME SA 240/SA 480, ASTM B 409/B 906, ASME SB 409/SB 906, BS 3072NA15, DIN 17460, EN 10028-7, EN 10095

Strip

AMS 5871, ASTM A 240/A 480, ASME SA 240/SA 480, ASTM B 409/B 906, ASME SB 409/SB 906, BS 3073NA15, DIN 17460, EN 10028-7, EN 10095

Pipe

ASTM B 407/B 829, ASME SB 407/SB 829 (Seamless Pipe), BS 3074NA15 (Seamless Pipe), DIN 17459

Tube

ASTM B 163, ASME SB 163 (Seamless Condenser & Heat Exchanger Tubes), ASTM B 407/B 829, ASME SB 407/SB 829 (Seamless Tube), ASTM B 515/B 751, 

ASME SB 515/SB 751 (Welded Tubes), 

BS 3074NA15 (Seamless Tubes), ISO 6207, DIN 17459

Other

ASTM B 366, ASME SB 366 (Fittings) - ASME Code Cases N201 & N254 (All products for nuclear construction), ISO 4955A (General), NACE MR-01-75, 

AFNOR Z5 NC 35-20, 

Werkstoff Nr 1.4876, UNS N08810, N08811

All

ASME Code Case 1325, SEW 470, VdTUV 412 and 434, Incoloy 800


The Incoloy 800 items which we can manufacture and supply are the followings.

Incoloy 800 Rod

3D printing spherical powder Incoloy 800

Incoloy 800 Rings, Forgings, pipe, tube, bars, plates, sheets, Strip, wire, fitting Union, Pipe Elbows, PIPE Tee, ADAPTERS, pipe bend, reducers, fitting caps, pipe outlets, Stub Ends, Couplings, pipe Nipples, BUSHINGS, pipes sockets, Pipe Gasket, pipe joints, pipe Cross, Pipe Wyes, seal ring, Flange, bolts, nuts, Rod

3D printing spherical powder Incoloy 825

Incoloy 825 Rings, Forgings, pipe, tube, bars, plates, sheets, Strip, wire, fitting Union, Pipe Elbows, PIPE Tee, ADAPTERS, pipe bend, reducers, fitting caps, pipe outlets, Stub Ends, Couplings, pipe Nipples, BUSHINGS, pipes sockets, Pipe Gasket, pipe joints, pipe Cross, Pipe Wyes, seal ring, Flange, bolts, nuts, Rod

Aircraft Steel 52100

Aircraft Steel 4620 Vac Melt

Aircraft Steel AMS 6440

Incoloy 925 Rod

3D printing spherical powder Incoloy 925

Incoloy 925 Rings, Forgings, pipe, tube, bars, plates, sheets, Strip, wire, fitting Union, Pipe Elbows, PIPE Tee, ADAPTERS, pipe bend, reducers, fitting caps, pipe outlets, Stub Ends, Couplings, pipe Nipples, BUSHINGS, pipes sockets, Pipe Gasket, pipe joints, pipe Cross, Pipe Wyes, seal ring, Flange, bolts, nuts, Rod

UNS N09901

Werkstoff Number 2.4662

BR HR 55

AMS 5660

AMS 5661

AECMA PrEN2176

AECMA PrEN2177

ISO 9723

ISO 9725

MSRR 7029, MSRR 7031 

Nimonic alloy 901 (tradename) 

UNS N19907

Incoloy Alloy 907 (tradename)

UNS N19909

AMS 5884 Bars, Forgings, Rings

AMS 5892 Sheet, Strip

AMS 5893 Bars, Forgings, Rings

Incoloy 909 (trademark)


ONE OF THE KIND, MILLIONS OF CHOICES

SUPERIOR QUALITY

PROMPT DELIVERY

FAVORABLE FEEDBACK

ALL AVAILABLE IN PESCO

SELECT PESCO, YOU WILL BE RIGHT


For more info and price of Incoloy 800, please send us inquiry and you will have quick reply soon.


Known as one of the professional manufacturers and suppliers of quality steel products, Petrol Steel Co.,Ltd is always at your service. Should you are interested in our High Temperature 3D Printing Spherical Powder Incoloy 800 Forgings Pipes Tubes Bars Plates Sheets Strips Wires Rods, you can check the mechanical properties, medical composition, hardness value and even the melting point with us first if you need. Now wholesale High Temperature 3D Printing Spherical Powder Incoloy 800 Forgings Pipes Tubes Bars Plates Sheets Strips Wires Rods in stock with our factory!

Hot Tags: High Temperature 3D Printing Spherical Powder Incoloy 800 Forgings Pipes Tubes Bars Plates Sheets Strips Wires Rods manufacturers, suppliers, factory, wholesale, in stock, melting point, mechanical properties, chemical composition, hardness value, incoloy 800
Related Products

Feedback

We're Here to Help

  • +86 13436334453 

    +86 13436334453

    JACKYWINN@FOXMAIL.COM

     A-4F, Wantone Center, A6, Chaowai St., Chaoyang Dist., Beijing, China

Newsletter

Enter in your email address to receive deals
and coupons.
Bookmark us today!