Inconel 625 (UNS N06625) is a nickel-chromium-molybdenum alloy with an addition of niobium. The addition of molybdenum acts with the niobium to stiffen the alloy matrix, providing a high strength without a strengthening heat treatment. The alloy resists a wide range of corrosive environments and has a good resistance to pitting and crevice corrosion.

Description

Nickel Alloy Inconel 625 3D printing spherical powder Forgings pipes tubes bars plates sheets Strips wires Rods


We are leading manufacturer and stockiest of Inconel 625 in China.


Inconel 625 Technical Data Sheet 


Inconel 625 Chemical Composition Limits

Weight %

Ni

Cr

Mo

Nb + Ta

Fe

Ti

C

Mn

Si

S

P

Al

Co

Alloy 625

58.0 min

20 - 23

8 -10

3.15 -4.15

5.0 max

0.40 max

0.10 max

0.50 max

0.50 max

0.15 max

0.15 max

0.40 max

1.0 max


Inconel 625 (UNS N06625) is a nickel-chromium-molybdenum alloy with an addition of niobium. The addition of molybdenum acts with the niobium to stiffen the alloy matrix, providing a high strength without a strengthening heat treatment. The alloy resists a wide range of corrosive environments and has a good resistance to pitting and crevice corrosion. Inconel 625 is used in chemical processing, aerospace and marine engineering oil & gas, pollution control equipment and nuclear reactors.


Inconel 625 Mechanical Properties


Material

Form and Condition

Tensile Strength MPa

Yield Strength (0.2% Offset) MPa

Elongation 4D(%)

Hardness HB

Ksi

MPa

Ksi

MPa

Alloy 625 Bar

Annealed

120

827

60

414

30

≤ 287 HB

Alloy 625 Sheet

Annealed

120

827

60

414

30

145-240

Alloy 625 Tube
     Seamless and Welded

Annealed

120

827

60

414

35

-


Inconel 625 Specifications

Bar

ASTM B 446, ASME SB 466, AMS 5666, ISO 9723, VdTUV 499, BS 3076 NA21, EN 10095, DIN 17752, ASME Code Case 1935

Rod

ASTM B 446, ASME SB 466, ISO 9723, VdTUV 499, BS 3076 NA21, EN 10095, DIN 17752, SME Code Case 1935

Wire

AMS 5837, ISO 9724, DIN 17753

Forging Stock

ASTM B 564, ASME SB 564, AMS 5666, ISO 9725, SME Code Case 1935, DIN 17754

Plate

ASTM B 443, ASME SB 443, AMS 5599, AMS 5869, MAM 5599, ISO 6208, VdTUV 499, BS 3072 NA21, EN 10095, DIN 17750, ASME Code Case 1935

Sheet

ASTM B 443, ASME SB 443, AMS 5599, AMS 5869, MAM 5599, ISO 6208, VdTUV 499, BS 3072 NA21, EN 10095, DIN 17750, ASME Code Case 1935

Strip

ASTM B 443, ASME SB 443, AMS 5599, AMS 5869, MAM 5599, ISO 6208, VdTUV 499, EN 10095, DIN 17750, ASME Code Case 1935

Pipe Seamless

ASTM B444, ASTM B829, ASME SB 444, ASME SB 829, BS3074 NA21

Pipe Welded

ASTM B705, ASTM B775, ASME SB 705, ASME SB 775

Tube Seamless

ASTM B444, ASTM B829, ASME SB 444, ASME SB 829, AMS 5581, BS3074 NA21, AMS 5581 Type 1

Tube Welded

ASTM B704, ASTM B751, ASME SB 704, ASME SB 704, AMS 5581, AMS 5581 Type 2

Tube

VdTUV 499, ISO 6207, DIN 17751, ASME Code Case 1935

Fittings

ASTM B 366, ASME SB 366

Other

UNS N06625, W. Nr 2.4856, ISO NW6625, NACE MR-01-75, INCONEL 625 (trademark), MSRR 7264


The Inconel 625 items which we can manufacture and supply are the followings.
Inconel 625 Rings, Forgings, pipe, tube, bars, plates, sheets, Strip, wire, fitting Union, Pipe Elbows, PIPE Tee, ADAPTERS, pipe bend, reducers, fitting caps, pipe outlets, Stub Ends, Couplings, pipe Nipples, BUSHINGS, pipes sockets, Pipe Gasket, pipe joints, pipe Cross, Pipe Wyes, seal ring, Flange, bolts, nuts, Rod

3D printing spherical powder Inconel 625

Inconel HX Rod

3D printing spherical powder Inconel HX

Inconel HX Rings, Forgings, pipe, tube, bars, plates, sheets, Strip, wire, fitting Union, Pipe Elbows, PIPE Tee, ADAPTERS, pipe bend, reducers, fitting caps, pipe outlets, Stub Ends, Couplings, pipe Nipples, BUSHINGS, pipes sockets, Pipe Gasket, pipe joints, pipe Cross, Pipe Wyes, seal ring, Flange, bolts, nuts, Rod

Alloy W Hastelloy W

UNS N10004

AMS 5755 Bar and Forgings

AMS 5786 Welding Wire


ONE OF THE KIND, MILLIONS OF CHOICES
 SUPERIOR QUALITY
 PROMPT DELIVERY
 FAVORABLE FEEDBACK
 ALL AVAILABLE IN PESCO
 SELECT PESCO, YOU WILL BE RIGHT


For more info and price of Inconel 625, please send us inquiry and you will have quick reply soon.


Known as one of the professional manufacturers and suppliers of quality steel products, Petrol Steel Co.,Ltd is always at your service. Should you are interested in our Nickel Alloy Inconel 625 3D Printing Spherical Powder Forgings Pipes Tubes Bars Plates Sheets Strips Wires Rods, you can check the mechanical properties, medical composition, hardness value and even the melting point with us first if you need. Now wholesale Nickel Alloy Inconel 625 3D Printing Spherical Powder Forgings Pipes Tubes Bars Plates Sheets Strips Wires Rods in stock with our factory!

Hot Tags: Nickel Alloy Inconel 625 3D Printing Spherical Powder Forgings Pipes Tubes Bars Plates Sheets Strips Wires Rods manufacturers, suppliers, factory, wholesale, in stock, melting point, mechanical properties, chemical composition, hardness value, inconel 625
Related Products

Feedback

We're Here to Help

  • +86 13436334453 

    +86 13436334453

    JACKYWINN@FOXMAIL.COM

     A-4F, Wantone Center, A6, Chaowai St., Chaoyang Dist., Beijing, China

Newsletter

Enter in your email address to receive deals
and coupons.
Bookmark us today!