Home > Products > Alloy Steel > Superalloys

Premium 3D Printing Spherical Powder Nickel Alloy Invar 36 Forgings Pipes Tubes Bars Plates Sheets Strips Wires Rods

For more info and price of Invar 36, please send us inquiry and you will have quick reply soon.

Description

Premium 3D Printing spherical powder Nickel Alloy Invar 36 Forgings pipes tubes bars Plates sheets Strips wires Rods


We are leading manufacturer and stockiest of Invar 36 in China.


Invar 36 Technical Data Sheet


Invar 36 Chemical Composition Limits

Weight %

Ni

Fe

C

Mn

P

S

Si

Cr

Mo

Co

Invar 36

35-38

Rem

0.10 max

0.06 max

0.025 max

0.025 max

0.35 max

0.50 max

0.50 max

1.0 max



Alloy 36 (NILO 36, INVAR 36) is a Nickel-Iron, low expansion alloy which contains 36% Nickel. Invar 36 has a low coefficient of expansion from cryogenic temperatures to about +500°F (260°C). Invar 36 also retains good strength and toughness at cryogenic temperatures. Common applications include tooling for aerospace composites, standards of length, measuring devices, thermostat rods, laser components and tanks and piping for the storage and transportation of liquefied gases.


Invar 36 Mechanical Properties


Material

Condition

Ultimate Tensile Strength

Yield Strength 0.2 %

Elongation (%)

 

 

psi

MPa

psi

MPa

 

Invar 36

Annealed

71,000

490

35,000

240

42


Invar 36 products

Invar 36 Tube is available the following size ranges.

Outside Diameter - 0.25mm (0.010") up to 16.00mm (0.625")

Wall - 0.05mm (0.002") up to 1.00mm (0.040")

Straight Lengths - 1.00mm (0.040") up to 5000.00mm (197")

Coils Lengths - 5 Meters to 15 Meters

Standard Tolerance- OD &ID +/-0.03mm (0.0012")

Wall +/- 10%

Tight Tolerance - OD&ID +/- 0.015mm (0.0006")

Wall +/-3%

Some thin wall tubes up to 25.40 mm (1.000") can be supplied.

Invar 36 Stock - Alloy 36

Invar 36 Round Bar

Invar 36 Plate

6.35 mm dia

6 mm THK

12.00 mm dia

10 mm THK

16.00 mm dia

13 mm THK

20.00 mm dia

19 mm THK

22.22 mm dia

25 mm THK

25.00 mm dia

30 mm THK

30.00 mm dia

40 mm THK

35.00 mm dia

50 mm THK

40.00 mm dia


45.00 mm dia


50.00 mm dia



Hot Rolled Plate Invar 36

Th


Width


Length

0.187"

X

72"

X

96"

0.250"

X

72"

X

96"

0.375"

X

72"

X

96"

0.500"

X

72"

X

96"

0.625"

X

70"

X

72"

0.750"

X

16"

X

100"

1.00"

X

16"

X

56"

1.50"

X

16"

X

46"

2.00"

X

20"

X

60"

2.50"

X

8.25"

X

51"

4.00"

X

7.125"

X

18.5"

4.625"

X

5"

X

51"

5.00"

X

12.7"

X

15.5"


Cold Rolled Sheet - Invar 36

Thickness


Width


Length

0.015

x

10.5

x

72

0.030

x

24

x

72

0.041

x

24

x

72

0.060

x

24

x

60

0.060

x

24

x

120

0.100

x

24

x

72

0.125

x

24

x

60

0.125

x

24

x

120


Invar Rod - Invar 36

Dia


Length

0.078

x

36

0.093

x

36

0.100

x

72

0.125

x

120

0.250

x

72

0.500

x

144

0.750

x

144

1.0

x

144

1.125

x

144

2.0



3.0



4.0




Invar Welding Wire - Invar 36

0.45

x

MIG Spools 25lb

0.096

x

36 TIG pkg'd in 10lb tubes

0.078

x

36 TIG

0.093

x

36 TIG


Invar 36 Specifications

UNS K93600, K93601

Werkstoff Nr. 1.3912

ASTM B 388, ASTM B 753, DIN 1715 (Sheet and Strip) 

ASTM F-1684

MIL-S-16598 and MIL-I-23011 CL 7

Trademarks - NILO 36 and INVAR 36

FeNi36


The Invar 36 items which we can manufacture and supply are the followings.

3D printing spherical powder Invar 36

Invar 36 Rod

Invar 36 Rings

Invar 36 Forgings

Invar 36 pipe

Invar 36 tube

Invar 36 bars

Invar 36 plates

Invar 36 sheets

Invar 36 Strip

Invar 36 wire

Invar 36 fitting Union

Invar 36 Pipe Elbows

Invar 36 PIPE Tee

Invar 36 ADAPTERS

Invar 36 pipe bend

Invar 36 reducers

Invar 36 fitting caps

Invar 36 pipe outlets

Invar 36 Stub Ends

Invar 36 Couplings

Invar 36 pipe Nipples 

Invar 36 BUSHINGS

Invar 36 pipes sockets

Invar 36 Pipe Gasket

Invar 36 pipe joints

Invar 36 pipe Cross

Invar 36 Pipe Wyes

Invar 36 seal ring

Invar 36 Flange

Invar 36 bolts

Invar 36 nuts


ONE OF THE KIND, MILLIONS OF CHOICES

SUPERIOR QUALITY

PROMPT DELIVERY

FAVORABLE FEEDBACK

ALL AVAILABLE IN PESCO

SELECT PESCO, YOU WILL BE RIGHT


For more info and price of Invar 36, please send us inquiry and you will have quick reply soon.


Known as one of the professional manufacturers and suppliers of quality steel products, Petrol Steel Co.,Ltd is always at your service. Should you are interested in our premium 3d printing spherical powder nickel alloy invar 36 forgings pipes tubes bars plates sheets strips wires rods, you can check the mechanical properties, medical composition, hardness value and even the melting point with us first if you need. Now wholesale premium 3d printing spherical powder nickel alloy invar 36 forgings pipes tubes bars plates sheets strips wires rods in stock with our factory!

Known as one of the professional manufacturers and suppliers of quality steel products, Petrol Steel Co.,Ltd is always at your service. Should you are interested in our Premium 3D Printing Spherical Powder Nickel Alloy Invar 36 Forgings Pipes Tubes Bars Plates Sheets Strips Wires Rods, you can check the mechanical properties, medical composition, hardness value and even the melting point with us first if you need. Now wholesale Premium 3D Printing Spherical Powder Nickel Alloy Invar 36 Forgings Pipes Tubes Bars Plates Sheets Strips Wires Rods in stock with our factory!

Hot Tags: Premium 3D Printing Spherical Powder Nickel Alloy Invar 36 Forgings Pipes Tubes Bars Plates Sheets Strips Wires Rods manufacturers, suppliers, factory, wholesale, in stock, melting point, mechanical properties, chemical composition, hardness value, invar 36
Related Products

Feedback

We're Here to Help

  • +86 159 0035 7871

    +86 159 0035 7871

    JACKYWINN@FOXMAIL.COM

     A-4F, Wantone Center, A6, Chaowai St., Chaoyang Dist., Beijing, China

Newsletter

Enter in your email address to receive deals
and coupons.
Bookmark us today!