Reliable 3D Printing Spherical Powder Inconel 725 Forgings Pipes Tubes Bars Plates Sheets Strips Wires Rods

Inconel 725 (UNS N07725) is a nickel-chromium-molybdenum-niobium alloy that is highly resistant to corrosion and has been age hardened for extremely high strength twice that of annealed alloy 625. Inconel 725 strength is developed by heat treatment rather than by cold work this also enables strength to be imparted to large non-uniform sections that cannot be strengthened by cold works.

Description

Reliable 3D printing spherical powder Inconel 725 Forgings pipes tubes bars plates sheets Strips wires Rods


We are leading manufacturer and stockiest of Inconel 725 in China.


Inconel 725 Technical Data Sheet


Inconel 725 Chemical Composition Limits

Weight%

Ni

Cr

Mo

Nb

Ti

Al

C

Mn

Si

P

S

Fe

Alloy 725

55.0-59.0

19.0 -22.5

7.0-9.5

2.75-4.0

1.0-1.7

0.35 max

0.03 max

0.35 max

0.20 max

0.015 max

0.010 max

Rem


Inconel 725 (UNS N07725) is a nickel-chromium-molybdenum-niobium alloy that is highly resistant to corrosion and has been age hardened for extremely high strength twice that of annealed alloy 625. Inconel 725 strength is developed by heat treatment rather than by cold work this also enables strength to be imparted to large non-uniform sections that cannot be strengthened by cold works. Inconel 725 is used for hangers, landing nipples and high strength fasteners in marine applications.


Inconel 725 Mechanical Properties


Material

Form and Condition

Yield Strength (0.2% Offset)

Tensile Strength

Elongation %

Hardness, Rc

 

 

ksi

MPa

ksi

MPa

 

 

Alloy 725 round

Annealed

62.0

427

124.0

855

57

5

Alloy 725 round

Age Hardened

133.0

917

180.0

1241

30

36

Transverse Specimens from hot-finished rounds of 4.0 to 7.5 in (102 to 190mm) diameter


Inconel 725 Specifications

Bar and Wire ASTM B 805, ASME Code Case 2217

Bar and Forging Stock SMC Specification HA91, ASME Code Case 2217

UNS N07725

FMC Spec M40504

NACE MR-0175/ ISO 15156 

Inconel 725 (trademark)

Alloy Nickel Alloy 706Inconel 706

Alloy Nickel Alloy 718Inconel 718

Alloy 722

Inconel 722

UNS N07722

AMS 5541 Sheet and Strip

AMS 5714 Bar and Forgings

UNS N07718

Werkstoff Nr 2.4668

AMS 5596 Sheet, Strip and Plate

AMS 5597 Sheet, Strip and Plate

AMS 5589 Seamless Tube

AMS 5590 Seamless Tube

AMS 5662 Bars, Forgings and Rings

AMS 5663 Bars, Forgings and Rings

AMS 5664 Bars, Forgings and Rings

AMS 5832 Welding Wire

ASTM B637 Forgings

ASTM B670 Plate, Sheet and Strip

AFNOR NC 19 Fe Nb, 

MSRR 7115 and MSRR 7116 

Inconel 718 (trademark) 

FMC Spec M40110, M40118, M40125, M40902, M40908, M40909, M40910

NACE MR-0175/ISO 15156 

UNS N09706

AMS 5701

AMS 5702

AMS 5703

Inconel 706 (tradename)


The Inconel 725 items which we can manufacture and supply are the followings.

Inconel 725 Rod

3D printing spherical powder Inconel 725

Inconel 725 Rings, Forgings, pipe, tube, bars, plates, sheets, Strip, wire, fitting Union, Pipe Elbows, PIPE Tee, ADAPTERS, pipe bend, reducers, fitting caps, pipe outlets, Stub Ends, Couplings, pipe Nipples, BUSHINGS, pipes sockets, Pipe Gasket, pipe joints, pipe Cross, Pipe Wyes, seal ring, Flange, bolts, nuts, Rod

Inconel X750 Rod

3D printing spherical powder Inconel X750

Inconel X750 Rings, Forgings, pipe, tube, bars, plates, sheets, Strip, wire, fitting Union, Pipe Elbows, PIPE Tee, ADAPTERS, pipe bend, reducers, fitting caps, pipe outlets, Stub Ends, Couplings, pipe Nipples, BUSHINGS, pipes sockets, Pipe Gasket, pipe joints, pipe Cross, Pipe Wyes, seal ring, Flange, bolts, nuts, Rod

ONE OF THE KIND, MILLIONS OF CHOICES

SUPERIOR QUALITY

PROMPT DELIVERY

FAVORABLE FEEDBACK

ALL AVAILABLE IN PESCO

SELECT PESCO, YOU WILL BE RIGHT


For more info and price of Inconel 725, please send us inquiry and you will have quick reply soon.


Known as one of the professional manufacturers and suppliers of quality steel products, Petrol Steel Co.,Ltd is always at your service. Should you are interested in our Reliable 3D Printing Spherical Powder Inconel 725 Forgings Pipes Tubes Bars Plates Sheets Strips Wires Rods, you can check the mechanical properties, medical composition, hardness value and even the melting point with us first if you need. Now wholesale Reliable 3D Printing Spherical Powder Inconel 725 Forgings Pipes Tubes Bars Plates Sheets Strips Wires Rods in stock with our factory!

Hot Tags: Reliable 3D Printing Spherical Powder Inconel 725 Forgings Pipes Tubes Bars Plates Sheets Strips Wires Rods manufacturers, suppliers, factory, wholesale, in stock, melting point, mechanical properties, chemical composition, hardness value, inconel 725
Related Products

Feedback

We're Here to Help

  • +86 159 0035 7871

    +86 159 0035 7871

    JACKYWINN@FOXMAIL.COM

     A-4F, Wantone Center, A6, Chaowai St., Chaoyang Dist., Beijing, China

Newsletter

Enter in your email address to receive deals
and coupons.
Bookmark us today!