Home > Products > Alloy Steel > Superalloys

Super Alloy Inconel 600 3D Printing Spherical Powder Forgings Pipes Tubes Bars Plates Sheets Strips Wires Rods

Inconel 600 (N06600) is a nickel-chromium-iron alloy with good oxidation resistance at high temperatures and resistance to chloride-ion stress corrosion cracking corrosion by high-purity water, and caustic corrosion. Inconel 600 also has excellent mechanical properties and has a desirable combination of high strength and good workability.

Description

Super Alloy Inconel 600 3D printing spherical powder Forgings pipes tubes bars plates sheets Strips wires Rods


We are leading manufacturer and stockiest of Inconel 600 in China.


Inconel 600 Technical Data Sheet


Inconel 600 Chemical Composition Limits

Weight%

C

S

Cr

Cu

Mn

Si

Ni

Fe

Nickel Alloy 600

0.15 max

0.015 max

14.0 - 17.0

0.50 max

1.0 max

0.50 max

72.0 min

6 - 10

Inconel 600 (N06600) is a nickel-chromium-iron alloy with good oxidation resistance at high temperatures and resistance to chloride-ion stress corrosion cracking corrosion by high-purity water, and caustic corrosion. Inconel 600 also has excellent mechanical properties and has a desirable combination of high strength and good workability. Used for furnace components, in chemical and food processing, in nuclear engineering and for the sparking electrodes.


Inconel 600 Mechanical Properties


Material

Form and Condition

Tensile Strength

Yield Strength

Elongation %

Hardness, Rockwell

 

 

ksi

MPa

ksi

MPa

 

 

Alloy 600 rod and bar

Cold drawn Annealed

80-100

550-690

25-50

170-345

55-35

65-85B

Alloy 600 Plate

Hot rolled Annealed

80-100

550-725

30-50

205-345

55-35

65-85B

Alloy 600 Sheet

Cold Rolled Annealed

80-100

550-690

30-45

205-310

55-35

88B max

Alloy 600 Tube and Pipe

Cold Drawn Annealed

80-100

550-690

25-50

170-345

55-35

88B max

Alloy 600 Wire

Cold Drawn Annealed

80-120

550-830

35-75

240-520

45-20

-

Alloy 600 Wire

Cold Drawn No 1 Temper

105-135

725-930

70-105

480-725

35-15

-

Alloy 600 Wire

Spring Temper

170-220

1170-1520

150-210

1035-1450

5-2

-

Inconel 600 Specifications

UNS N06600

W. Nr 2.4816

AMS 5540 Sheet, Strip and Plate

AMS 5665 Bar, Forgings and Rings

AMS 5580 Seamless Tubing 

ASTM B168 Plate

ASTM B166 Bar

ASTM B167 Seamless Pipe

ASTM B163 Seamless Tube

ASTM B517 Weld Pipe

ASTM B516 Weld Tube

ASTM B564 Forging

MIL N 22986

MIL N 23338

MIL N 6710

QQ W 390

MIL N 15721

MIL N 22987

MIL N 23229

MIL N 6840

NA14

Inconel 600 (Trademark)

Nickel Alloy 617

Nickel Alloy 601

Inconel 601

UNS N06617

ASTM B 166

WS 2.4663a 

ASME SB-166, Boiler Code Sections I, VIII,

SAE AMS 5887, SAE AMS 5888 and SAE AMS 5889

Inconel 617 ®

UNS N06601

ASTM B168 Plate

ASTM B166 Bar

ASTM B167 Seamless Pipe

ASTM B163 Seamless Tube

ASTM B564 Forgings

DIN 17752

AMS 5715 Bar, Forgings and Rings

AMS 5870 Sheet, Strip and Plate

Inconel 601 ®


The Inconel 600 items which we can manufacture and supply are the followings.

3D printing spherical powder Inconel 600

Inconel 600 Rings, Forgings, pipe, tube, bars, plates, sheets, Strip, wire, fitting Union, Pipe Elbows, PIPE Tee, ADAPTERS, pipe bend, reducers, fitting caps, pipe outlets, Stub Ends, Couplings, pipe Nipples, BUSHINGS, pipes sockets, Pipe Gasket, pipe joints, pipe Cross, Pipe Wyes, seal ring, Flange, bolts, nuts, Rod

Aircraft Steel AISI 4140

Inconel C276 Rod

3D printing spherical powder Incoloy C276

Inconel C276 Rings, Forgings, pipe, tube, bars, plates, sheets, Strip, wire, fitting Union, Pipe Elbows, PIPE Tee, ADAPTERS, pipe bend, reducers, fitting caps, pipe outlets, Stub Ends, Couplings, pipe Nipples, BUSHINGS, pipes sockets, Pipe Gasket, pipe joints, pipe Cross, Pipe Wyes, seal ring, Flange, bolts, nuts, Rod


ONE OF THE KIND, MILLIONS OF CHOICES

SUPERIOR QUALITY

PROMPT DELIVERY

FAVORABLE FEEDBACK

ALL AVAILABLE IN PESCO

SELECT PESCO, YOU WILL BE RIGHT


For more info and price of Inconel 600, please send us inquiry and you will have quick reply soon.


Known as one of the professional manufacturers and suppliers of quality steel products, Petrol Steel Co.,Ltd is always at your service. Should you are interested in our Super Alloy Inconel 600 3D Printing Spherical Powder Forgings Pipes Tubes Bars Plates Sheets Strips Wires Rods, you can check the mechanical properties, medical composition, hardness value and even the melting point with us first if you need. Now wholesale Super Alloy Inconel 600 3D Printing Spherical Powder Forgings Pipes Tubes Bars Plates Sheets Strips Wires Rods in stock with our factory!

Hot Tags: Super Alloy Inconel 600 3D Printing Spherical Powder Forgings Pipes Tubes Bars Plates Sheets Strips Wires Rods manufacturers, suppliers, factory, wholesale, in stock, melting point, mechanical properties, chemical composition, hardness value, inconel 600
Related Products

Feedback

We're Here to Help

  • +86 13436334453 

    +86 13436334453

    JACKYWINN@FOXMAIL.COM

     A-4F, Wantone Center, A6, Chaowai St., Chaoyang Dist., Beijing, China

Newsletter

Enter in your email address to receive deals
and coupons.
Bookmark us today!